The difference between martensitic stainless steel and austenitic stainless steel:
The main alloying element in martens stainless steel is chromium. It is usually used in weakly corrosive media, such as seawater, freshwater, and water vapor, with a usage temperature of than or equal to 580 degrees Celsius. It is typically used as a material for parts and tools under high stress. Due to its poor weldability it is generally not used as a welded piece. The main alloying elements in austenitic stainless steel are chromium and nickel. This type of steel has high, low brittle transition temperature, good corrosion resistance, high-temperature strength, excellent oxidation resistance, and good pressure processing and welding performance.
Detailed introduction to martens stainless steel: A type of stainless steel whose mechanical properties can be adjusted through heat treatment, commonly known as a hardenable stainless steel. The typical grades are Cr3 types, such as 2Cr13, 3Cr13, and 4Cr13. It has high hardness after quenching and different tempering temperatures result in different combinations of strength and toughness. It is mainly used in steam turbine blades, tableware, and surgical instruments. Based on difference in chemical composition, martensitic stainless steel can be divided into martensitic chromium steel and martensitic chromium-nickel steel. Based on the and strengthening mechanism, it can also be divided into martensitic stainless steel, martensitic and semi-austenitic (or semi-martensitic precipitation hardening stainless steel, and martensitic aging stainless steel.
Detailed introduction to austenitic stainless steel: It refers to stainless steel that has an austitic structure at room temperature. When the steel contains about 18% Cr, 8%~10% Ni, and about 0.1%, it has a stable austenitic structure. Austenitic chromium-nickel stainless steel includes the well-known 18Cr-8Ni steel and high Cr-Ni series steel developed by increasing the Cr and Ni content and adding Mo, Cu, Si, Nb, Ti, etc. Austenitic stainless is non-magnetic and has high toughness and plasticity, but its strength is low. It cannot be strengthened through phase transformation, only through cold working. If, Ca, Se, Te, etc., are added, it has good machinability.