Welding characteristics of duplex stainless steel

May 07, 2024 Leave a message

After normal solid solution treatment (heating at 1020 ℃ to 1100 ℃ and water cooling), duplex stainless steel contains approximately 50% to 60% austenite and 50% to 40% ferrite structure. As the heating temperature increases, the proportion of the two phases does not change significantly.
Dual phase stainless steel has good low-temperature impact toughness, such as a 20mm thick transverse specimen with an impact absorption energy of over 100J at -80 ℃. In most media, it has good resistance to uniform corrosion and point corrosion. However, it should be noted that this type of steel, when heat treated below 950 ℃, is prone to corrosion due to σ The precipitation of phases will significantly deteriorate their stress corrosion resistance. Due to the appropriate ratio of Cr equivalent to Ni equivalent in the steel, a large amount of primary austenite structure is still retained after high-temperature heating, and secondary austenite can be generated during the cooling process. As a result, the total amount of austenite phase in the steel is not less than 30% to 40%, which makes the steel have good intergranular corrosion resistance.