I. Introduction to stainless steel:
All metals react with oxygen in the atmosphere to form an oxide film on the surface. Unfortunately, the iron oxide formed on ordinary carbon steel continues to oxidize, causing the corrosion to expand continuously and eventually form holes. The surface of carbon steel can be protected by painting or electroplating with oxidation-resistant metals (such as zinc, nickel, and chromium). However, as people know, this protection is only a thin film. If the protective layer is damaged, the steel below will begin to rust.
Steel that resists weak corrosive media such as air, steam, and water and chemical corrosive media such as acids, alkalis, and salts. Also known as stainless acid-resistant steel. In practical applications, steel that resists weak corrosive media is often called stainless steel, while steel that resists chemical media is called acid-resistant steel. Due to the chemical composition differences between the two, the former may not necessarily resist chemical media corrosion, while the latter generally has stainless properties. The corrosion resistance of stainless steel depends on the alloy elements contained in the steel. Chromium is the basic element that enables stainless steel to obtain corrosion resistance. When the chromium content in steel reaches about 12%, chromium reacts with oxygen in the corrosive medium and forms a very thin oxide film (passive film) on the steel surface, which can prevent the steel matrix from further corrosion. In addition to chromium, commonly used alloy elements also include nickel, molybdenum, titanium, niobium, copper, nitrogen, etc., to meet the requirements of stainless steel structure and performance for various applications.
II. Classification of stainless steel: Stainless steel is usually classified according to matrix structure as follows:
- Ferritic stainless steel. Contains 12% - 30% chromium. Its corrosion resistance, toughness, and weldability increase with the increase of chromium content. It has better resistance to chloride stress corrosion than other types of stainless steel.
- Austenitic stainless steel. Contains more than 18% chromium and about 8% nickel and a small amount of molybdenum, titanium, nitrogen and other elements. It has good comprehensive performance and can resist corrosion from various media.
- Austenitic-ferritic duplex stainless steel. It has the advantages of both austenitic and ferritic stainless steel and has superplasticity.
- Martensitic stainless steel. It has high strength but poor plasticity and weldability.
III. Characteristics and uses of stainless steel:
IV. Stainless steel surface treatment processes:
V. Packaging characteristics and main products of various steel mills:
Domestic other steel mills: Shandong Taigang, Jiangyin Zhaoshun, Xinghua Dainan, Xi'an Huaxin, Southwest, and Dongfang Special Steel. These small factories mainly process rerolled plates from waste materials. Their production processes are backward, the plate surfaces are poor, there is no guarantee of mechanical properties. The element content is almost the same as that of large factories, but the price is cheaper than the same model of large factories.
Foreign imported steel mills: Shanghai Krupp, South Africa, North America, Japan, Belgium, Finland. Imported plates have advanced production processes, neat and beautiful plate surfaces, and cut edges. The price is higher than that of domestic models of the same type.
VI. Specifications, models, and sizes of stainless steel: Stainless steel plates include coils and original flat plates.
- Coils are divided into cold-rolled coils and hot-rolled coils, trimmed coils and untrimmed coils.
- The thickness of cold-rolled coils is generally 0.3 - 3mm. There are also cold-rolled plates with a thickness of 4 - 6mm. The widths are 1m, 1219m, and 1.5m, denoted by 2B.
- The thickness of hot-rolled coils is generally 3 - 14mm. There is also a coil with a thickness of 16mm. The widths are 1250, 1500, 1800, and 2000, denoted by NO.1.
- Coils with widths of 1.5m, 1.8m, and 2.0m are trimmed coils.
- The widths of untrimmed coils are generally 1520, 1530, 1550, 2200, etc., which are wider than the normal width.
- In terms of price, the same model of trimmed coils and untrimmed coils generally have a price difference of about 300 - 500 yuan.
- Coils can be custom-cut according to the length required by customers. After being flattened by a leveling machine, they are called flattened plates. For cold rolling, it is generally flattened to 1m * 2m, 1219 * 2438, also called 4 * 8 feet. For hot rolling, it is generally flattened to 1.5m * 6m, 1.8m * 6m, 2m * 6m. Plates opened according to these sizes are called standard plates or fixed-size plates.
Original flat plates are also called single-pass rolled plates: - The thickness of original plates is generally between 4mm and 80mm. There are also 100mm and 120mm thicknesses, and this thickness can be custom-ordered.
- The widths are 1.5m, 1.8m, and 2m, and the length is more than 6 meters.
- Characteristics: Original flat plates are large in volume, high in cost, difficult to pickle, and inconvenient to transport.
VII. Thickness distinction:
- Due to the slight deformation of the rolling rolls caused by heating during the rolling process in the steel mill, the thickness of the rolled plates shows deviation, generally thicker in the middle and thinner on both sides. When measuring the plate thickness, it is stipulated by the state that the middle part of the plate head should be measured.
- The reason for the tolerance is based on market and customer needs. Generally, it is divided into large tolerance and small tolerance.
VIII. Specific gravity of various stainless steel materials:
- The specific gravity of 304, 304L, 304J1, 321, 201, and 202 is 7.93.
- The specific gravity of 316, 316L, 309S, and 310S is 7.98.
- The specific gravity of the 400 series is 7.75.
IX. Calculation formulas for stainless steel:
Calculation formulas:
Stainless steel pipe: (outer diameter - wall thickness) × wall thickness × 0.02491 = Kg/m
Stainless steel plate; thickness * (width × length) × specific gravity = Kg/square centimeter
Round steel: (diameter × diameter) × 0.00623 = Kg/M
Coil price: flat plate price * theoretical thickness/actual thickness - leveling fee
Flat plate price: coil price * actual thickness/theoretical thickness + leveling fee
Theoretical calculation formula:
Coil plate: weighed weight ÷ reference thickness (actual thickness) × theoretical thickness = theoretical weight
Flattened plate of coil plate: length × width × thickness × density = theoretical weight
Medium plate: length × width × theoretical thickness × density = theoretical weight
Coil length: actual weight ÷ width ÷ thickness (reference thickness) ÷ density = coil length
Actual thickness of coil: trimmed coil = coil weight ÷ width ÷ coil length ÷ density
Untrimmed coil = (coil weight - edge wire weight) ÷ width ÷ coil length ÷ density
Flat plate price: flat plate price = (coil weight * market base price - edge wire amount + leveling fee) / total weight of flattened plate
Explanation of some terms in the stainless steel industry:
- Overweight plate:
Reason: Due to technical reasons in the steel mill, when rolling thick plates, the actual thickness is thicker than the standard thickness, or the length and width are longer than the standard, resulting in a weight heavier than the theoretical weight.
Quotation method: Add 200 - 400 yuan/ton to the daily quotation, or quote to the customer according to the weighed price to make up for the overweight part. - Rerolled plate:
Rerolled plates are generally made by small factories from waste materials and billets. The processing technology is backward, the plate surface is poor, there is no guarantee of quality and mechanical properties, and the nickel content does not meet the formal requirements. In processing, it is difficult to drill holes and bend wires. Its advantage is that the price is about 1500 - 2000 yuan cheaper than that of large factories. Rerolled plates are generally produced in Dainan. - Cold-rolled plate:
Reason for producing cold-rolled plates: Because there is a large price difference between hot-rolled coils and cold-rolled coils, and rerolled coils are cheaper than cold-rolled coils, cold-rolled plates have price advantages and large profit margins, so many manufacturers produce cold-rolled plates.
Production process: Manufacturers that produce cold-rolled plates do not have the ability to produce cold-rolled plates themselves. Their production processes do not meet the requirements for producing cold plates. So they buy hot-rolled coils from large steel mills, perform surface annealing and heat treatment, and then reroll them into cold-rolled coils of various thicknesses.
Characteristics: First-grade materials are produced without any flaws. Second-grade materials may cause scratches and color differences during production, but they are not very serious. There is no substantial difference in mechanical properties and element content compared to first-grade materials. The price is relatively cheaper than that of first-grade materials. It can be used by customers with less strict requirements! - Difference between L1 and LH in 201:
L1 means that the nickel content in the 201 plate reaches 0.8%; LH means that the nickel content in the 201 plate reaches 0.6%. The price of LH is relatively cheaper than that of L1.
Uses and properties of various types of stainless steel:
Precipitation hardening stainless steel. It has good formability and weldability and can be used as an ultra-high-strength material in the nuclear industry, aerospace industry. According to the composition, it can be divided into Cr series (SUS400), Cr-Ni series (SUS300), Cr-Mn-Ni (SUS200) and precipitation hardening series (SUS600). 200 series - chromium-nickel-manganese austenitic stainless steel 300 series.
Precipitation hardening stainless steel. It has good formability and weldability and can be used as an ultra-high-strength material in the nuclear industry, aerospace industry.
According to the composition, it can be divided into Cr series (SUS400), Cr-Ni series (SUS300), Cr-Mn-Ni (SUS200) and precipitation hardening series (SUS600).
200 series - chromium-nickel-manganese austenitic stainless steel
300 series - chromium-nickel austenitic stainless steel
301 - Good ductility, used for molded products. Can also be hardened by mechanical speed. Good weldability. Better wear resistance and fatigue strength than 304 stainless steel.
302 - Same corrosion resistance as 304. Due to relatively higher carbon content, it has better strength.
303 - By adding a small amount of sulfur and phosphorus, it is easier to machine.
304 - That is, 18/8 stainless steel. The GB grade is 0Cr18Ni9.
309 - Has better temperature resistance than 304.
316 - After 304, it is the second most widely used steel type. Mainly used in the food industry and surgical instruments. Adding molybdenum elements gives it a special anti-corrosion structure. Due to its better resistance to chloride corrosion than 304, it is also used as "shipbuilding steel". SS316 is usually used in nuclear fuel recovery devices. 18/10 grade stainless steel usually also meets this application level. [1]
Model 321 - Except for adding titanium elements to reduce the risk of weld corrosion of the material, other properties are similar to 304.
400 series - ferrite and martensitic stainless steel
408 - Good heat resistance, weak corrosion resistance, 11% Cr, 8% Ni.
409 - The cheapest model (in Britain and the United States), usually used as automobile exhaust pipes, belongs to ferrite stainless steel (chromium steel).
410 - Martensitic (high-strength chromium steel), good wear resistance, poor corrosion resistance.
416 - Adding sulfur improves the processing performance of the material.
420 - "Tool grade" martensitic steel, similar to the earliest stainless steel such as Buehler high chromium steel. Also used for surgical knives and can be made very shiny.
430 - Ferrite stainless steel, for decorative purposes, such as for automotive accessories. Good formability, but poor temperature resistance and corrosion resistance.
440 - High-strength tool steel with slightly higher carbon content. After proper heat treatment, it can obtain higher yield strength. The hardness can reach 58HRC and belongs to the hardest stainless steel. The most common application example is "razor blade". There are three commonly used models: 440A, 440B, 440C. In addition, there is 440F (easy-to-process type).
500 series - heat-resistant chromium alloy steel.
600 series - martensitic precipitation hardening stainless steel.
630 - The most commonly used precipitation hardening stainless steel model, usually also called 17-4; 17% Cr, 4% N.
Common stainless steel surface treatment technologies have the following treatment methods:
① Surface natural whitening treatment; ② Surface mirror bright treatment; ③ Surface coloring treatment.
1.3.1 Surface natural whitening treatment: During the processing of stainless steel, through processes such as coiling, hemming, welding, or artificial surface heating treatment, black oxide scale is generated. This hard gray-black oxide scale mainly consists of two EO4 components, NiCr2O4 and NiF. In the past, strong corrosive methods such as hydrofluoric acid and nitric acid were generally used to remove it. However, this method has high cost, pollutes the environment, is harmful to the human body, and has strong corrosiveness. It has been gradually eliminated. Currently, there are mainly two methods for treating oxide scale:
(1) Sandblasting (shot blasting) method: Mainly use the method of spraying micro glass beads to remove the black oxide scale on the surface.
(2) Chemical method: Use a pollution-free pickling and passivation paste and a cleaning solution with inorganic additives that is non-toxic at room temperature for immersion washing. Thus, the purpose of whitening treatment of stainless steel's natural color is achieved. After treatment, it basically looks like a matte color. This method is more suitable for large and complex products.
1.3.2 Stainless steel surface mirror bright treatment methods: According to the complexity of stainless steel products and user requirements, mechanical polishing, chemical polishing, and electrochemical polishing methods can be used to achieve mirror gloss. The advantages and disadvantages of these three methods are as follows:
1.3.3 Surface coloring treatment: Stainless steel coloring not only gives stainless steel products various colors, increases the variety of products, but also improves the wear resistance and corrosion resistance of products.
There are the following coloring methods for stainless steel:
(1) Chemical oxidation coloring method;
(2) Electrochemical oxidation coloring method;
(3) Ion deposition oxide coloring method;
(4) High-temperature oxidation coloring method;
(5) Gas phase cracking coloring method.
A brief overview of various methods is as follows:
(1) Chemical oxidation coloring method: In a specific solution, the color of the film is formed by chemical oxidation. There are dichromate method, mixed sodium salt method, sulfidation method, acidic oxidation method, and alkaline oxidation method. Generally, the "INCO method" is used more. However, if you want to ensure consistent color of a batch of products, a reference electrode must be used for control.
(2) Electrochemical coloring method: In a specific solution, the color of the film is formed by electrochemical oxidation.
(3) Ion deposition oxide coloring method chemical method: Place the stainless steel workpiece in a vacuum coating machine for vacuum evaporation plating. For example, watch cases and watch straps plated with titanium gold are generally golden yellow. This method is suitable for processing large quantities of products. Because the investment is large and the cost is high, it is not cost-effective for small batch products.
(4) High-temperature oxidation coloring method: In a specific molten salt, immerse the workpiece and maintain it at certain process parameters to make the workpiece form an oxide film of a certain thickness and present various colors.
(5) Gas phase cracking coloring method: It is relatively complex and is less used in industry.